Skip to content
  • Testimonials
  • Factory Tour
  • Hindi
    • English
    • Japanese
    • French
    • German
    • Italian
    • Spanish
    • Swedish
    • Irish
    • Dutch
    • Portuguese
    • Korean
    • Greek
    • Turkish
    • Vietnamese
    • Thai
    • Indonesian
    • Malay
    • Danish
    • Finnish
    • Hindi
    • Hebrew
    • Icelandic
    • Romanian
    • Russian
DT 3D Printing New Logo

DT 3d printing service

OEM manufacturer – SLM (Metal 3D Printing) Specialists

  • Home
  • Metal 3D Printing Service
  • CNC Machining
    • CNC Turning
    • CNC Milling
    • CNC Post-processing
  • Material Guide
        • Plastic 3D Printing Materials
          • Resin (ABS-Like, PC-Like)
          • Nylon (PA6, PA12, TPU)
          • Red Wax
          • PLA, TPU, PA, Carbon Fiber, PC
        • Metal 3D Printing Materials
          • Aluminum Alloy (6061 / AlSi10Mg / 7075)
          • Stainless Steel (316L / 304L / 17-4 / 347)
          • Titanium Alloy (TC4 / TA1)
          • Mold Steel (S136/HB/CX/1.2709)
          • Nickel-rich Alloy (GH4169 / GH3128 / INCONEL625)
          • Brass Alloy (CuCrZr / Tin Bronze)
        • Metal Materials for CNC
          • Aluminum / Alloy / Titanium / Nickel
          • Stainless Steel / Tool Steel / Alloy Steel
          • Carbon Steel / Brass / Copper / Bronze
        • Plastic Materials for CNC
          • ABS / Acrylic / Delrin / Nylon / PP
          • HDPE / PE / PC / PEI / ULTEM
          • PEEK / POM / TECAFORMAH
  • Other Service
        • Industry Solutions
          • Mold / Mould
          • Aerospace
          • Car Manifolds
          • Car Parts
          • Motorcycle Parts
          • Titanium Bike
          • Robotics
          • Art Crafts / Gifts
        • Plastic & Resin 3D Printing
          • SLA (Stereolithography)
          • SLS (Selective Laser Sintering)
          • DLP (Digital Light Processing)
          • FDM (Fused Deposition Modeling)
          • MJF (Multi Jet Fusion)
          • BJ (Binder Jetting)
        • Post-Processing Services
          • CNC Finish Machining
          • Surface Finishing
          • Anodizing
          • Electroplating
          • Heat treatment
          • HIP (Hot Isostatic Pressing)
        • Blog
          • Metal 3D Printing + CNC Machining
          • 3D Printing Business Ideas
          • SLM 3D Printing Guide
          • Custom 3D Printed Sculptures
          • 3D Print Motorcycle Parts
          • Metal 3D Printed Impellers
          • Used 3D Printers Guide
  • Testimonials
  • About DT
    • Factory Tour Video
    • VR Factory Tour
  • Contact us

Industrial SLM Metal 3D Printing Materials Available: Aluminum Alloy / Stainless Steels / Titanium Alloy / Mold Steel / Copper Alloy / Nickel-based Superalloy

DT's Workers in Front of Our SLM Metal 3D Printers
The Industrial SLM Metal 3D Printers in DT Factory
The High-Precision Industrial SLS 3D Printers in DT Factory
MaterialStainless Steel
Grade316L
Main CompositionFe: bal
Cr: 16~18%
Ni: 10~14%
Mo: 2~3%
Physical PropertiesPowder Particle Size15-53 μm
Flowability (s/50g)16~18
Tap Density (g/cm³)4.5~4.7
Apparent Density (g/cm³)4.0~4.2
DensityDensity7.9
Sample Theoretical Density>99%
As-built PropertiesHardness13~15HRC
Tensile Strength/Rm580MPa
Yield Strength/Rp0.2490MPa
Elongation at Break/A32%
Reduction of Area/Z/
Elastic Modulus/E/
Heat-treated PropertiesHardness13~15HRC
Tensile Strength/Rm670MPa
Yield Strength/Rp0.2550MPa
Elongation at Break/A35%
Reduction of Area/Z45%
Elastic Modulus/E185GPa
MaterialStainless Steel
Grade17-4PH
Main CompositionFe: bal
Cr: 15.5~17.5%
Ni: 3~5%
Cu: 3~5%
Physical PropertiesPowder Particle Size5-53 μm
Flowability (s/50g)16~18
Tap Density (g/cm³)4.5~4.7
Apparent Density (g/cm³)4.0~4.2
DensityDensity7.9
Sample Theoretical Density>99%
As-built PropertiesHardness18~22HRC
Tensile Strength/Rm860MPa
Yield Strength/Rp0.2700MPa
Elongation at Break/A19%
Reduction of Area/Z/
Elastic Modulus/E/
Heat-treated PropertiesHardness32~42HRC
Tensile Strength/Rm1340MPa
Yield Strength/Rp0.21210MPa
Elongation at Break/A13%
Reduction of Area/Z/
Elastic Modulus/E/
MaterialMold Steel
Grade18Ni300
Main CompositionFe: bal
Ni: 17~19%
Co: 8.5~9.5%
Mo: 4.5~5.2%
Physical PropertiesPowder Particle Size15-53 μm
Flowability (s/50g)19.3
Tap Density (g/cm³)4.8~4.9
Apparent Density (g/cm³)4.2~4.5
DensityDensity8.09
Sample Theoretical Density>99%
As-built PropertiesHardness38 ~42 HRC
Tensile Strength/Rm1177MPa
Yield Strength/Rp0.2980MPa
Elongation at Break/A8%
Reduction of Area/Z40%
Elastic Modulus/E113GPa
Heat-treated PropertiesHardness54-57HRC
Tensile Strength/Rm2163MPa
Yield Strength/Rp0.21920MPa
Elongation at Break/A2.50%
Reduction of Area/Z10%
Elastic Modulus/E125GPa
MaterialTitanium Alloy
GradeTC4
Main CompositionTi: bal
Al: 5.5~6.75%
V: 3.5~4.5%
Physical PropertiesPowder Particle Size15-53 μm
Flowability (s/50g)36~40
Tap Density (g/cm³)2.7~2.85
Apparent Density (g/cm³)2.3~2.5
DensityDensity4.56
Sample Theoretical Density>99%
As-built PropertiesHardness380HV
Tensile Strength/Rm1000MPa
Yield Strength/Rp0.2950MPa
Elongation at Break/A7%
Reduction of Area/Z/
Elastic Modulus/E105GPa
Heat-treated PropertiesHardness350HV
Tensile Strength/Rm1000
Yield Strength/Rp0.2825
Elongation at Break/A14%
Reduction of Area/Z/
Elastic Modulus/E125GPa
MaterialAluminum Alloy
GradeAlSi10Mg
Main CompositionAl: bal
Si: 9.0~11%
Mg: 0.2~0.45%
Physical PropertiesPowder Particle Size15-53 μm
Flowability (s/50g)150
Tap Density (g/cm³)1.55
Apparent Density (g/cm³)1.3~1.45
DensityDensity2.7
Sample Theoretical Density≥99.3%
As-built PropertiesHardness/
Tensile Strength/Rm420MPa
Yield Strength/Rp0.2240MPa
Elongation at Break/A5.50%
Reduction of Area/Z/
Elastic Modulus/E44GPa
Heat-treated PropertiesHardness/
Tensile Strength/Rm330MPa
Yield Strength/Rp0.2210MPa
Elongation at Break/A11.00%
Reduction of Area/Z/
Elastic Modulus/E/
MaterialAluminum Alloy (Anodized)
Grade6061
Main CompositionAl: bal
Mg: 0.8~1.2%
Si: 0.4~0.8%
Physical PropertiesPowder Particle Size15-53 μm
Flowability (s/50g)120
Tap Density (g/cm³)1.5
Apparent Density (g/cm³)1.2
DensityDensity2.7
Sample Theoretical Density≥98%
As-built PropertiesHardness/
Tensile Strength/Rm290MPa
Yield Strength/Rp0.2250MPa
Elongation at Break/A14%
Reduction of Area/Z/
Elastic Modulus/E/
Heat-treated PropertiesHardness/
Tensile Strength/Rm/
Yield Strength/Rp0.2/
Elongation at Break/A/
Reduction of Area/Z/
Elastic Modulus/E/
MaterialCopper Chromium Zirconium Alloy
GradeCuCrZr
Main CompositionCu: bal(≥98%)
Cr: 0.5~1.5%
Zr: 0.05~0.25%
Physical PropertiesPowder Particle Size15-53 μm
Flowability (s/50g)18~22
Tap Density (g/cm³)5.2
Apparent Density (g/cm³)4.0~4.4
DensityDensity8.9
Sample Theoretical Density≥99.3%
As-built PropertiesHardness90HV
Tensile Strength/Rm350MPa
Yield Strength/Rp0.2250MPa
Elongation at Break/A30%
Reduction of Area/Z/
Elastic Modulus/E/
Heat-treated PropertiesHardness90HV
Tensile Strength/Rm543MPa
Yield Strength/Rp0.2432 MPa
Elongation at Break/A21%
Reduction of Area/Z/
Elastic Modulus/EConductivity IACS: ≥85%
MaterialTin Bronze Alloy
GradeCuSn10
Main CompositionCu: bal
Sn: 9.0~11%
Zn: 0.5%
Physical PropertiesPowder Particle Size15-53 μm
Flowability (s/50g)16
Tap Density (g/cm³)5.8
Apparent Density (g/cm³)4.2~4.8
DensityDensity8.64
Sample Theoretical Density≥98%
As-built PropertiesHardness150HV
Tensile Strength/Rm578MPa
Yield Strength/Rp0.2470MPa
Elongation at Break/A23.90%
Reduction of Area/Z/
Elastic Modulus/E/
Heat-treated PropertiesHardness/
Tensile Strength/Rm/
Yield Strength/Rp0.2/
Elongation at Break/A/
Reduction of Area/Z/
Elastic Modulus/E/
MaterialNickel-based Superalloy
GradeGH4169
Main CompositionNi: 50~55%
Cr: 17~21%
Fe: bal
 
Physical PropertiesPowder Particle Size
Flowability (s/50g)14
Tap Density (g/cm³)4.9
Apparent Density (g/cm³)4.41
DensityDensity8.24
Sample Theoretical Density≥99%
As-built PropertiesHardness220HV
Tensile Strength/Rm1158MPa
Yield Strength/Rp0.2914MPa
Elongation at Break/A14%
Reduction of Area/Z/
Elastic Modulus/E/
Heat-treated PropertiesHardness/
Tensile Strength/Rm/
Yield Strength/Rp0.2/
Elongation at Break/A/
Reduction of Area/Z/
Elastic Modulus/E/

We own dozens of SLM 3D printers for industrial use.
And the main commonly used metallic materials are these:

  • Aluminum Alloy (6061 / AlSi10Mg / 7075)
  • Stainless Steel (316L / 304L / 17-4 / 347)
  • Titanium Alloy (TC4 / TA1)
  • Mold Steel (S136/HB/CX/1.2709)
  • Nickel-rich Alloy (GH4169 / GH3128 / INCONEL625)
  • Brass Alloy (CuCrZr / Tin Bronze)

DT is a one – stop 3D printing platform.
Not only because we have dozens of SLM 3D printers and plastic 3D printers, but also, we have invested in 6 3D – printing and CNC machining related factories.

So if you have personalized requirements regarding materials and want to have customized solutions, you can contact us directly.

Customer Support
FAQ
Free 3D Drawing Modification
Free Custom 3D Drawing (Limited Availability)

Legal Statements
Shipping Policy
Return and Refund Policy
Privacy Statement
Terms of Service
Imprint
Disclaimer
Cookie Policy

About us
Factory Tour Video
Blog
Cooperation
About DT
Contact

YouTube Twitter TikTok Facebook Instagram Quora LinkedIn Pinterest Reddit Medium


Copyright © 2026 DT 3d printing service
All Rights Reserved.


Manage Cookie Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}
Manage Cookie Consent
To provide the best experiences, we use technologies like cookies to store and/or access device information. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}